- Barrier Coating
CURE TIME:
- Pot life (100 grams cupful):
- At 25°C: 20 to 30 minutes
- Working time (thin film):
- At 25°C: 90 to 110 minutes
- Solid state:
- At 25°C: 9 to 12 hours
*Epoxy cures faster at higher temperatures and in thicker applications.
CURE TEMP:
- Minimum recommended temperature: 16°C
PRODUCT SIZES:
- Junior: 100g
- 206-A: 0.2kg
- 206-B: 1kg
- 206-C: 5kg
- 206-E: 45kg
*These sizes are 206 hardener sizes ONLY and exclude resin sizes
206 Slow Hardener® Facts
QUICK LINKS Helpful Tips, Safety Guidelines, Manuals, and More:
BONDING & CLAMPING
There are two types of structural bonding with epoxy. Two-step bonding is the preferred method for most situations because it promotes maximum epoxy penetration into the bonding surface and prevents epoxy-starved joints. Single-step bonding can be used when joints have minimal loads and excess absorption into porous surfaces is not a problem.