Wood Rot Repair Kit

Restore Compromised Wood with Confidence.

 

New from WEST SYSTEM® Epoxy, the Wood Rot Repair Kit provides a cost-effective and time-saving solution for making structurally sound repairs to rotted wood. This two-part, solvent-free epoxy system penetrates deep into damaged areas and restores by consolidating weakened wood fibres. It’s formulated to be flexible enough to move with the wood’s natural movement, preventing issues from cracking.

Whether you’re restoring a boat, garden houses, home projects or delamination on your Campervan, Wood Rot Repair Epoxy is the solution that makes rotted wood structurally sound for years to come.

  • COMPATIBLE WITH FILLERS
    • When mixed with WEST SYSTEM Fillers, it creates a thickened epoxy perfect for filling large voids or rebuilding missing sections of wood.
  • PREVENTS CRACKING
    • Designed to have a bit of flex, Wood Rot epoxy accommodates natural wood movement without cracking.
  • 100% SOLID
    • Wood Rot Epoxy is 100% solid, meaning it’s formulated without solvents. Other penetrating epoxies containing solvents are susceptible to shrinkage and may cause unwanted voids, making your repair less structurally sound.
WEST SYSTEM| image: Wood rot medium kit render (1)

PROJECT USES:

  • Wood components
  • Home exterior
  • Campervan repairs
  • Marine
  • Decorative trim
  • Woodworking

CURE TIME:

When working in a 22°C environment:

  • Working time: 30-40 minutes
  • Recoat time: thin film: ≥ 12 hours. Surface build-up: 3 hours
  • Time to sand: 24 hours

CURE TEMP:

  • Recommended temp: 22°C
  • Minimum temp: 10°C

PRODUCT SIZES:

  • Small kit (360ml): 240ml resin, 120ml hardener
  • Medium kit (1.5L): 1000ml resin, 500ml hardener
  • Large kit (6L): 4L resin, 2L hardener

Wood Rot Repair Kit Facts