What quantity of epoxy do I need?

To determine the quantity of WEST SYSTEM Epoxy needed to coat a given area, use this handy quantity table.

West System 105 resin and 205 fast hardener

Resin VolumeHardener VolumeTotal MixedPorous Surfaces
(saturation coat)
Non-porous Surfaces
(build-up coat)
101 Mini 250g50g300g1.95-2.25m²2.55-2.85m²
104 Junior 500G100g600g3.9-4.5m²5.1-5.7m²
105-A 1 kg205-A or 206-A
0.2kg
1.2kg7.8-9m²10-11.5m²
105-A 1kg207-A or 209-A
0.29kg
1.29kg9-10.5m²11.5-13m²
105-B 5kg205-B or 206-B
1kg
6kg39-45m²51-57m²
105-B 5kg207-B or 209-B
1.45kg
6.45kg45-51.5m²58-64.5m²
105-C 25kg205-C or 206-C
5kg
30kg195-225m²225-285m²
105-C 25kg207-C or 209-C
7.2kg
32.2kg225.5-257.5m²290-322m²
105-E 225kg205-E or 206-E
45kg
270kg1755-2025m²2295-2565m²
105-E 225kg207-E or 209-E
64.5kg
289.5kg2026.5-2316m²2605.5-2895m²

Estimating epoxy quantity and coverage

It’s important to have a good idea of how much epoxy your project is going to need before you start. You want to be sure you have enough to hand for the job – but equally, you don’t want to spend money on epoxy that you don’t need. Hear more from our expert here.